Property | Ocr21A16Nb | Ocr27A17Mo2 |
---|---|---|
C (Carbon) | 0.05 | 0.05 |
P (Phosphorus) | 0.025 | 0.025 |
S (Sulfur) | 0.025 | 0.025 |
Mn (Manganese) | 0.7 | 0.7 |
Cr (Chromium) | 21.00~23.00 | 26.50~27.80 |
Ni (Nickel) | ≤0.60 | ≤0.60 |
Al (Aluminum) | 5.00~7.00 | 6.00~7.00 |
Mo (Molybdenum) | / | 1.80~2.20 |
Nb (Niobium) | 0.5 | / |
Maximum Operating Temperature (℃) | 1380 | 1450 |
Density (g/cm³) | 7.1 | 7.1 |
Technical Parameters | ||||||
Parameter | 1200℃ | 1400℃ | 1600℃ | 1700℃ | 1800℃ | 1900℃ |
Maximum Operating Temperature | 1200℃ | 1400℃ | 1600℃ | 1700℃ | 1800℃ | 1900℃ |
Long-term Operating Temperature | 1150℃ | 1350℃ | 1550℃ | 1680℃ | 1780℃ | 1850℃ |
Temperature Control Range | 100-1200℃ | 100-1400℃ | 100-1600℃ | 100-1700℃ | 100-1800℃ | 100-1900℃ |
Temperature Control Precision | ±1℃ | ±1℃ | ±1℃ | ±1℃ | ±1℃ | ±1℃ |
Temperature Measuring Element | K-type thermocouple | S-type thermocouple | B-type thermocouple | B-type thermocouple | B-type thermocouple | Thermocouple + optical fiber |
Heating Element Material | High-temperature alloy resistance wire | Silicon carbide rod | Molybdenum disilicide rod | 1800-type molybdenum disilicide rod | 1850-type molybdenum disilicide rod | 1900-type molybdenum disilicide rod |
Installation Position of Heating Elements | Three-sided heating (both sides + bottom) | Top/bottom / both sides | Both sides | Both sides | Both sides | Both sides
|